Kovar and Invar are two highly regarded materials in the manufacturing industry, particularly for creating sensitive electronic equipment. While both are known for their low thermal expansion and high strength, they each offer distinct advantages that make them suited for specific applications. Recognizing the distinctions among these substances can assist you in deciding which is most suitable for your requirements.
CHY Product Page
What is Kovar?
Kovar, also known as ASTM F15, is a nickel-cobalt ferrous alloy renowned for its compatibility with borosilicate glass due to its similar coefficient of thermal expansion. This property makes Kovar an excellent choice for sealed electronic components, such as metal-ceramic packages. Additionally, Kovar offers outstanding machinability, allowing it to be developed into complex shapes with tight tolerances. It also provides good thermal shock and chemical corrosion resistance, making it ideal for applications like electrical housings and optical reflectors.
Applications of Kovar:
Electronic packages
Vacuum-sealed devices
Airtight containers
Transistors
Ceramic mountings
When considering Kovar for your project, keep in mind that Kovar plates are often used in manufacturing processes that require precise and durable components. These plates are particularly valued for their stability and resistance in demanding environments.
What is Invar?
Invar is an iron-nickel alloy composed of nearly equal amounts of nickel and iron. It is best known for its negligible coefficient of thermal expansion, which makes it an excellent choice for applications that demand high precision and stability across a wide range of temperatures. Invars properties make it ideal for scientific instruments, clocks, and other precision devices where thermal expansion could cause significant errors.
Applications of Invar:
Scientific instruments
Precision optical devices
Telescope mirrors
Interferometers
Electronic devices
Physical Properties:
Kovar has a thermal expansion coefficient of 4.57 x 10^-6 m/mK, closely matching that of borosilicate glass, making it suitable for glass-to-metal seals. In contrast, Invar has a much lower coefficient of 1.2 x 10^-6 m/mK, making it excellent for applications where thermal stability is critical.
Kovars melting point is °C, and its density is kg/m³, while Invars is slightly lower, at °C and at kg/m³.
Kovar and Invar are ferromagnetic but differ in magnetic behaviour. Kovar exhibits a strong magnetic response, whereas Invar is magnetically soft, meaning it has lower coercivity and hysteresis.
Processing:
Kovar is relatively easy to machine using oil-based lubricants and water-soluble cutting fluids. It can be formed through cold or hot rolling, pressing, and forging. Invar, on the other hand, is more challenging to use due to its hardness and toughness. It often requires precise control during forming methods like spinning or stamping to maintain dimensional stability.
Cost:
Generally, Kovar is more cost-effective than Invar. Invars precise composition and manufacturing process contribute to its higher price. However, the cost difference may be justified depending on the applications specific requirements.
Conclusion
Kovar and Invar offer unique properties suitable for different industrial applications. Kovars low thermal expansion and minimal outgassing make it an excellent choice for electronic packages, vacuum-sealed devices, and other applications where these properties are crucial. In contrast, Invars exceptional thermal stability makes it the material of choice for precision optical devices and scientific instruments.
When deciding between Kovar and Invar, consider your applications specific needs, including physical properties, processing methods, and cost. By doing so, you can select the material that best meets your requirements, ensuring optimal performance and longevity in your project.
The metals world in observed the centennial of the discovery of the low expansion alloy known as Invar (UNS K). This remarkable alloy has been so important to scientific advancement that it earned the Nobel Prize in for its inventor, Charles-Edouard Guillaume, the first and only scientist in history to be so honored for a metallurgical achievement.
Still exhibiting the "Invar Effect" that defies understanding, Invar has bred an entire family of low expansion, nickel-iron alloys that are used today in a wide variety of both commonplace and high technology applications. Commercial uses have proliferated in fields as diverse as semiconductors, television, information technology, aerospace and cryogenic transport.
Guillaume, employed by the International Bureau of Weights and Measures, was looking in for a metal for geodesic tapes and wires that would not change in length when exposed to temperature variations. In addition, he wanted a cost-effective material for reference bars of perfectly defined length that could be used as secondary standards throughout the world.
He had many heats of nickel-iron alloys melted, handicapped often by feed stock that was contaminated. In the process, experimenting with nickel contents of 30% to 60%, Guillaume discovered that the coefficient of expansion at room temperature was lowest at a nickel level of 36%.
With 36% nickel, in fact, the alloy exhibited the least amount of thermal expansion of any alloy known. Since Guillaume considered the expansion of his new alloy "invariable", it eventually became known as Invar.
Guillaume published a graph similar to Fig. 1 visualizing the unique thermal expansion behavior of an "Invar-Effect" alloy. The expansion characteristic of these nickel-iron alloys is broadly determined by ferromagnetism.
These alloys exhibit very low expansivity below their Curie temperature (the temperature below which they are ferromagnetic). This low thermal expansivity anomaly, often referred to as the "Invar Effect", is related to spontaneous volume magnetostriction where lattice distortion counteracts the normal lattice thermal expansivity.
Above the Curie temperature, 36% nickel and other nickel-iron alloys expand at a high rate because they are no longer ferromagnetic. A number of theories have been proposed to explain this phenomenon. Although these theories have provided some insight, the mechanism is not yet sufficiently understood.
For more information, please visit INvar Material.
Once the 36% nickel and its companion nickel-iron alloys were discovered, it didn't take long to find applications that could utilize their low thermal expansivity. Surveying tapes and wires, as well as pendulums for grandfather clocks became important early applications. Nickel-iron alloys were substituted for platinum for glass sealing wire at great cost savings in the 's. They also were used in light bulbs and electronic vacuum tubes for radios.
Uses expanded further in the 's. Nickel-iron alloys were used as one of the bimetals in thermostats for temperature control. A copper-coated 42% nickel-balance iron alloy was being used in the lead-in seals of incandescent lights. A 56% nickel alloy was used to make measuring devices for testing gauges and machine parts.
World War II greatly increased the demand for "Invar Effect" nickel-iron alloys, particularly by the military. Demand escalated dramatically for alloys used in vacuum tubes and other products in the fast growing electronics industry.
Applications continued to spread in the prosperous 's and 's. The 36% nickel and other nickel-iron alloys were needed for low expansion components in bimetals for circuit breakers, motor controls, TV temperature compensating springs, appliance and heater thermostats, aerospace and automotive controls, heating and air conditioning, etc.
Glass-to-metal and ceramic-to-metal seals were in great demand. Since several of the "Invar-Effect" nickel-iron alloys had thermal characteristics similar to those of glass and ceramics, they were the natural choice for such applications. They were also used for the sealing needs of semi-conductors and microprocessors. These include pin feed-throughs, packaging and lid seals.
The demand for thermostat metals continued to grow in the 's and 's. The 36% nickel alloy has been found quite useful for containers used to transport liquid natural gas on tankers. The alloy minimizes cryogenic shrinkage.
A 36% nickel-iron alloy has been used more recently for shadow masks in high-definition CRT (television) tubes. It has been used for this application in Japan and Europe as a solution to the "doming effect" of the shadow mask. In the U. S., the 36% nickel alloy with a high expansion alloy has been used in deflection springs which reposition the mask to the color phosphors.
Newer applications use nickel-iron alloys for structural components in precision laser and optical measuring systems, and wave guide tubes. These alloys have been used in microscopes, in support systems for giant mirrors in telescopes and in a variety of scientific instruments requiring mounted lenses.
36% nickel-balance iron alloys have been used for composite molds by the aerospace industry. New generation aircraft, in particular, need 36% nickel-balance iron alloys for molds that will hold tight dimensional tolerances while advanced composites are cured at moderately high temperatures. The "Invar-Effect" family of alloys, in fact, is helping to raise modern science to higher levels with applications in orbiting satellites, lasers, ring laser gyroscopes and a host of high-tech applications.
Nature of Expansivity As shown in Fig. 1, the thermal expansion curve for "Invar-Effect" alloys consists of a low expansivity portion and a high expansivity portion. Below their Curie Temperature, these alloys are magnetic and their expansivities are anomalously low. Above it, they expand at a normal, high rate. This high rate extends to the melting point of the alloy. It can be noticed that there is a transition range between the low expansion and high expansion components. This transition is evidently related to the deterioration of ferromagnetism as the alloy approaches the Curie Temperature
Below room temperature, these alloys have low expansivity. Below approximately liquid nitrogen temperature (-196°C), their expansivity declines to near zero. The low expansion portion of the curve is most important because its slope defines the coefficient of expansion, and its length describes the useful temperature range of low expansivity.
Inflection temperature can be determined by a slope intercept method. It is the temperature at which the slopes taken from the low expansivity and the high expansivity curve portions of the expansion curve intersect. Measuring the Curie Temperature is laborious. Whereas, the inflection temperature can be determined simply from expansion curves.
In his early investigations, Guillaume learned how variations in nickel content affect the coefficient of expansion of the nickel-iron alloys. He found that expansion reached a minimum with 36% nickel (Fig. 2), and that on either side of this value the expansion coefficient increased dramatically.
Alloys with nominally less than 36% nickel are seldom used for controlled expansion applications primarily for two reasons: (a) these alloys can transform to martensite, which drastically increases the expansivity, and (b) they have low Curie Temperatures, which reduce the temperature range over which they may be used. Therefore, the alloys with 36% or more nickel are usually considered for controlled expansion applications.
All of the alloys in the Invar family are nickel-iron or nickel-iron-cobalt alloys, and all exhibit face-centered cubic crystal structure. As nickel content increases from 36%, thermal expansivity and Curie Temperature also increase. Curie Temperature increases from 280°C (536°F) for 36% nickel to greater than 565°C (°F) for 50% nickel.
The 36% nickel alloy's low coefficient of expansion, along with its off-the-shelf availability, make it one of the most commonly used materials for applications requiring low expansivity. But, depending on the temperature range of interest, it may not be entirely suitable for some applications. Although it exhibits the lowest thermal expansivity, it also has the lowest Curie Temperature. That limits its useful temperature range.
For applications around ambient temperature requiring the lowest expansivity, the 36% nickel is the obvious choice. It has been the most widely used nickel-iron alloy in applications such as electronic devices where dimensional changes due to temperature must be minimal, for structural members in precision optical measuring devices, and as the low expansion side in bimetal thermostats.
For certain applications, however, other alloys in the Invar family may be more suitable. In each case, alloy selection should take into account the temperature range for the intended application, as well as the coefficient of expansion desired over that range. The relative expansion rates for the "Invar-Effect" alloys are shown in Fig. 3.
Two alloys in this family (Fig. 4) have been found suitable for unique low expansion requirements. FCarpenter Technology Free-Cut Invar "36"® alloy (UNS K), with a slight increase in expansion properties, has been shown to offer improved machinability for applications where high parts productivity is important. This alloy has been used for aircraft controls and a variety of electronic devices
The second alloy - Carpenter Technology Super Invar "32-5" - is an iron-nickel-cobalt alloy which exhibits approximately one half the thermal of Carpenter Technology Invar "36"® alloy at or near room temperature. It has been used for structural components and supports for optical and laser instruments.
Fig. 4 - Typical properties and chemical composition of the Invar family of alloys.
Any one of four other nickel-iron alloys may be particularly suitable for service in higher temperature ranges. For example, Low Expansion "39" alloy (ASTM B-753) has a useful low thermal expansivity extending to approximately 250°C (482°F). It has been used as the low expansion element in thermostat bimetal products.
Carpenter Technology Glass Sealing 42 alloy, sometimes known as 42 alloy (ASTM F-30), has been commonly used for hermetic sealing to certain glasses. It is also has been used for high reliability ceramic- and plastic-sealed semiconductor packages.
Carpenter Technology Low Expansion "42"® thermostat alloy (ASTM B-753) has a virtually constant low rate of thermal expansion at temperatures up to about 350°C (662°F), while Low Expansion "45" alloy (ASTM B-753) has a relatively constant rate of thermal expansion to about 450°C (842°F). Both metals have been used in thermostats and thermoswitches. The thermal expansivity of the higher-nickel alloy approximates the thermal expansivity of alumina ceramics over certain temperature ranges. The alloy in this family with the highest nickel content, Carpenter Technology Glass Sealing "52" alloy (ASTM F-30) has been used for glass sealing of certain "soft" glasses.
The entire group of "Invar-Effect" nickel-iron alloys machine similar to, but not as well as a Carpenter Technology 316 austenitic stainless steel. They are readily machinable, although they are soft and do produce gummy chips. Therefore, large, sharp and rigidly supported tooling is recommended, with slower speeds. Where high productivity and good surface finish are important, a big edge goes to the Carpenter Technology Free-Cut Invar "36" alloy, the free-machining alloy variation.
All of the alloys in the family are very ductile, thus readily cold headed and formed. Stamping from cold-rolled strip is easily accomplished. Parts may be deep drawn from properly annealed strip.
Fabrication does add stresses which, unrelieved, can change the thermal expansion behavior. When that happens, parts placed in service as fabricated may not meet design requirements. To prevent such incident, annealing and stress relieving thermal treatments may be needed to promote structural uniformity and dimensional stability.
After severe forming, bending and machining, relief of stresses induced by these operations can be accomplished by annealing at temperatures of 760°C (°F) to 980°C (°F) long enough to thoroughly heat through the section. However, nickel-iron alloys will oxidize readily at these high temperatures.
When annealing cannot be done in a non-oxidizing atmosphere (vacuum, dry hydrogen, dissociated ammonia, argon, etc.), sufficient material must be present to allow cleaning by light grinding, pickling, etc., after annealing. For sections having light finishing cuts or grinding performed after annealing, stress relief is accomplished by heating to 315°C (600°F) to 425°C (800°F) long enough to uniformly heat through the work piece.
Invar is a critical alloy that has endured for more than a century. It is in a league of its own, having grown in importance over the years and given life to a stream of new technologies.
The group of "Invar-Effect" alloys represents a significant, growing volume in today's specialty metals universe. Below their Curie Temperatures, these alloys exhibit anomalously low thermal expansivities. A minimum in low thermal expansivity is reached at approximately 36% nickel. Increasing the nickel content increases the thermal expansivity and also raises the Curie temperature.
Collectively, this family of nickel-iron alloys has been found suitable for a host of applications that require different expansivities over a broad temperature range. Because of the widespread and growing demand for their special properties, these alloys seem likely to make an even greater contribution to modern science as they begin their second century on Earth.
***
By Leslie L. Harner, Product Application Manager, Electronic & Magnetic Alloys
Carpenter Technology Corporation
Reading, PA
USA